. 2009 May 29;15(11):3331–3340. doi: 10.1089/ten.tea.2008.0369

FIG. 3.

FIG. 3.

Image of a BVS during mechanical testing with markers to track local displacement to determine local strains (a). Outer diameter of a BVS cultured under cyclic pressure application (32.5 ± 7.5 mmHg, rate of one cycle per minute) and no axial stretching (b). Data were collected once per minute for 96 h. Scale bar = 500 μm. Color images available online at www.liebertonline.com/ten.