Skip to main content
. 2007 Jan 18;4(14):439–461. doi: 10.1098/rsif.2006.0196

Figure 7.

Figure 7

Temperature-dependent conductivity as measured on metallically boron-doped CVD diamond. The doping level is in the range of 5×1020 B cm−3. σ is activated with 2 meV, which indicates a hopping process of holes in the acceptor band.